After TPU material changeover, burnt spots persist for a long time
Análise das causas
TPU residual material is retained and degraded in dead corners; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry literature and should be confirmed first during troubleshooting
Solução
Use purging material to thoroughly replace during changeover; empty the barrel before shutdown; periodically disassemble and clean; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
TPU changeover cleaning must be thorough plus disassembled cleaning; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future