Uneven color when EAA is mixed with color masterbatch
Fenómeno do problema
EAA/color masterbatch injection molded products show color streaks and areas of uneven color depth
Análise das causas
The carrier resin of the color masterbatch is incompatible with EAA; poor dispersion of the color masterbatch, pigment agglomeration; unstable melt flow during '2079851475616104452 causes pigment orientation
Solução
1) Select EAA or similar carrier color masterbatch to ensure compatibility; 2) Twin-screw extrusion pelletizing for pre-dispersion; 3) Appropriately extend the mixing time to ensure pigment dispersion; 4) Reduce the injection speed to reduce pigment orientation
Conclusão principal
Carrier matching of the color masterbatch and full dispersion are the key to color uniformity