Voltar a Problema e solução
Extrusion & Post 13 visualizações

Gel particles in EAA extruded film

Fenómeno do problema
Transparent gel particles of 0.1-0.5mm appear on the surface of EAA extruded film
Análise das causas
High molecular weight components in EAA are not fully melted during extrusion, forming local highly crystalline regions; extrusion temperature too low or insufficient mixing
Solução
1) Raise the extrusion temperature by 5-10°C to ensure full melting; 2) Increase the length of the screw mixing section; 3) Inspect the raw material to ensure consistent grade; 4) Replace with a finer 120-mesh screen to intercept unmelted particles
Conclusão principal
Gel particles are caused by insufficient melting; raising the temperature and mixing are the key
EAA film gel particle melting temperature mixing section high molecular weight component