Insufficient EAA toughness, brittle fracture
Fenómeno do problema
EAA product elongation at break <50%, brittle fracture without yielding
Análise das causas
EAA molecular weight too low, insufficient toughness foundation; excessive crosslinking losing toughness; coarse crystallization increasing brittleness
Solução
1) Select high molecular weight EAA to improve toughness; 2) Control crosslinking degree to avoid excess; 3) Use nucleating agent to refine crystallization and improve toughness
Conclusão principal
Insufficient toughness is caused by low molecular weight and coarse crystallization; selecting high MW is key