Poor EAA plasticization

Fenómeno do problema
Unmelted particles appearing in EAA products, incomplete plasticization
Análise das causas
Insufficient screw compression ratio <2.5, low plasticizing pressure; screw speed too low, insufficient shear; processing temperature too low
Solução
1) Select a screw with compression ratio >3; 2) Increase screw speed to increase shear; 3) Increase processing temperature by 5-10°C
Conclusão principal
Poor plasticization is caused by improper screw design; optimizing the screw and raising temperature is key