Menu
Materiais Máquinas
Perspetivas
Artigos Vídeos Problema e solução
About
Sobre a Chembull Parceiros de média
Contacte-nos
Idioma
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Voltar a Problema e solução
Processing Machinery 7 visualizações

EEA Purging Difficulty

Fenómeno do problema
EEA purging requires 2-3h, time-consuming, affecting changeover efficiency
Análise das causas
EEA has strong adhesion, forming a firm adhesive layer on the screw and barrel; EEA has poor thermal stability, becoming sticky at high temperature and harder to remove
Solução
1) Before purging, flush with high-viscosity PE to carry away EEA residue; 2) Lower the purging temperature below the EEA softening point to reduce adhesion; 3) Use dedicated purging compound
Conclusão principal
Purging difficulty is caused by the strong adhesion of EEA; PE flushing and temperature reduction are key
EEA purging difficulty adhesion PE flushing dedicated purging compound

Isto foi útil?

0 pessoas acharam isto útil

ChemAI