Material Analysis 14 visualizações

Unstable shrinkage rate of EMA

Fenómeno do problema
The shrinkage rate of EMA products fluctuates ±0.8%, exceeding the ±0.2% requirement
Análise das causas
Molecular weight differences between EMA batches cause shrinkage rate variation; processing temperature fluctuation affects crystallinity and thereby shrinkage rate
Solução
1) Strictly control raw material batch consistency; 2) Stabilize processing temperature within ±2°C to ensure consistent crystallinity; 3) Reserve adjustment space for mold shrinkage compensation
Conclusão principal
Unstable shrinkage rate is caused by batch differences and temperature fluctuation; raw material and temperature control are key
EMA shrinkage rate batch difference stable temperature control crystallization consistency