Injection Molding
6 visualizações
Obvious EMA surface color difference
Fenómeno do problema
Color shades vary at different parts of EMA products with color difference ΔE>5
Análise das causas
Color masterbatch granules unevenly dispersed; pigment orientation during injection causes uneven color distribution; barrel temperature fluctuation causes color change
Solução
1) Use color masterbatch masterbatch method to ensure uniform dispersion; 2) Reduce injection speed to reduce pigment orientation; 3) Stabilize barrel temperature within ±2°C
Conclusão principal
Color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key
Isto foi útil?
0 pessoas acharam isto útil