Extrusion & Post 12 visualizações

EMA surface snakeskin texture

Fenómeno do problema
Snakeskin-like irregular texture on EMA extruded product surface
Análise das causas
Extrusion temperature too low with uneven melt elastic recovery; uneven die temperature distribution
Solução
1) Increase extrusion temperature to the processing temperature range; 2) Homogenize die temperature within ±2°C; 3) Reduce extrusion rate to reduce elastic recovery
Conclusão principal
Snakeskin texture is caused by low temperature extrusion and elastic recovery; raising temperature and reducing speed are key
EMA snakeskin texture extrusion temperature elastic recovery die temperature control