Blow Molding 5 visualizações

Severe parison sag in EVA extrusion '2079851475616104457

Fenómeno do problema
EVA extrusion '2079851475616104457 parison sag of 20-40mm causes bottle bottom wall thickness of only 0.3-0.4mm
Análise das causas
EVA melt strength low with parison stretched thin under gravity; parison extrusion speed slow increasing sag time; parison temperature too high with low viscosity worsening sag
Solução
1) Add slight crosslinking agent 0.3-0.5wt% to increase melt strength; 2) Increase parison extrusion speed to shorten sag time; 3) Lower parison temperature by 10-15°C to increase viscosity; 4) Wall thickness controller to compensate sag
Conclusão principal
Parison sag is caused by low melt strength; slight crosslinking and wall thickness control are key
EVA '2079851475616104457 parison sag melt strength slight crosslinking wall thickness control