Unstable dimensions in EVA extrusion

Fenómeno do problema
EVA extruded product cross-section dimensions fluctuate ±10% with periodic changes along the length
Análise das causas
Unstable feeding amount with feeding screw speed fluctuation; extrusion temperature periodically fluctuating ±5°C; haul-off speed not matching extrusion speed
Solução
1) Use loss-in-weight feeder to ensure stable feeding; 2) PID control of each extruder zone temperature with ±1°C precision; 3) Closed-loop control of haul-off speed linked with extrusion speed; 4) Control processing temperature at 140-200±5°C
Conclusão principal
Extrusion dimensional stability depends on feeding precision, temperature control and haul-off synchronization