Extrusion & Post 13 visualizações

Severe screw wear of EVA extruder

Fenómeno do problema
After 200h of EVA extrusion, screw and barrel wear reaches 0.5mm
Análise das causas
Filler causes large wear on screw; screw material hardness insufficient without nitriding; processing temperature too high causing EVA to adhere to screw and worsen wear
Solução
1) Use nitrided screw or bimetallic screw SK-2 alloy; 2) Lower processing temperature to reduce adhesive wear; 3) Treat filler with coupling agent to reduce friction; 4) Regularly check wear and replace promptly when >0.3mm
Conclusão principal
Screw wear is caused by filler friction and adhesion; wear-resistant screw and temperature control are key
EVA extrusion screw wear nitrided screw filler friction bimetallic screw