Injection Molding 6 visualizações

EVOH and color masterbatch mixing with uneven color

Fenómeno do problema
EVOH/color masterbatch injection molded products show color streaks and areas of inconsistent color depth
Análise das causas
Color masterbatch carrier resin incompatible with EVOH; poor color masterbatch dispersion with pigment agglomeration; unstable melt flow during '2079851475616104452 causing pigment orientation
Solução
1) Select EVOH or similar carrier color masterbatch to ensure compatibility; 2) Twin-screw extrusion pelletizing for pre-dispersion; 3) Appropriately extend mixing time to ensure pigment dispersion; 4) Reduce injection speed to reduce pigment orientation
Conclusão principal
Color masterbatch carrier matching and sufficient dispersion are the key to color uniformity
EVOH coloring color masterbatch carrier compatibility pigment dispersion color streaks