Injection Molding 1 visualizações

EVOH '2079851475616104452 Cold Slug Marks

Fenómeno do problema
EVOH injection molded products show cold slug marks near the gate
Análise das causas
Nozzle temperature too low causing residual material from the previous shot to cool and solidify in the nozzle; cold slug well design insufficient to hold cold material; injection pressure insufficient
Solução
1) Increase nozzle temperature to 190-230°C; 2) Mold design with sufficiently large cold slug well; 3) Ensure fresh melt at the nozzle front before each shot; 4) Increase injection pressure to push cold material through the gate
Conclusão principal
Cold slug marks are caused by solidified residual material in the nozzle; increasing nozzle temperature and cold slug well design are key
EVOH injectioncold slug marknozzle temperaturecold slug wellinjection pressure