Snakeskin pattern on PU surface
Fenómeno do problema
Snakeskin-like irregular texture on the surface of PU extruded products
Análise das causas
Extrusion temperature too low, uneven melt elastic recovery; uneven die temperature distribution
Solução
1) Increase extrusion temperature to the processing temperature range; 2) Homogenize die temperature ±2°C; 3) Reduce extrusion rate to reduce elastic recovery
Conclusão principal
Snakeskin pattern is caused by low-temperature extrusion and elastic recovery; raising temperature and reducing speed are key