Irregular deformation of the product after demolding

Fenómeno do problema
Irregular deformation of the product after demolding, flat areas become curved, dimensions out of tolerance, warpage direction related to uneven shrinkage
Análise das causas
Uneven product wall thickness, large shrinkage differences in all directions Uneven mold cooling, temperature difference causing shrinkage differences Insufficient injection pressure or uneven holding Improper gate position, unbalanced flow causing orientation differences Product temperature too high at demolding, insufficient rigidity, deformation
Solução
Optimize wall thickness design to be as uniform as possible Improve cooling water channel layout to make mold temperature uniform Increase holding pressure to ensure compaction in all directions Adjust gate position to balance flow Lower mold temperature to the low side of 40-80°C, extend cooling
Conclusão principal
Warpage needs to be addressed from wall thickness uniformity, cooling uniformity and flow balance
warpagedeformationuneven shrinkagecooling