Injection Molding 1 visualizações

Wave-like lines appear on the product surface

Fenómeno do problema
Wave-like lines appear on the product surface, periodically distributed along the flow direction, affecting appearance and feel
Análise das causas
Unstable injection speed causes melt front fluctuation Improper gate type produces turbulence Mold temperature too low (below the lower limit of 40-80°C), the melt front cools quickly Improper holding pressure switchover timing Raw material fluidity fluctuation
Solução
Stabilize injection speed, avoid sudden fast and slow Change the gate type, e.g., from pin gate to fan gate Appropriately increase the mold temperature to the 40-80°C range Optimize the holding pressure switchover point Ensure the raw materials are uniformly mixed
Conclusão principal
Surface waviness requires stable injection speed and mold temperature
wavinessflow instabilitymold temperatureinjection speed