CEF extrusion film has gel spots
Fenómeno do problema
The CEF extruded film has transparent gel spots of 0.2-1mm
Análise das causas
CEF residual crosslinked gel; the processing temperature is too high and local crosslinking occurs
Solução
1) Low gel content CEF; 2) Processing ≤220°C to avoid thermal crosslinking; 3) Screen 80-120 mesh interception
Conclusão principal
CEF gel spots are caused by residual crosslinking; raw material control and filtration are the key