Extrusion & Post 13 visualizações

Material Hang-up and Carbon Deposits on CMC Extrusion Die

Fenómeno do problema
After CMC extrusion shutdown, a brown carbon deposit layer is found on the inner wall of the die, and after restarting, black specks appear on the product surface
Análise das causas
CMC is heated for a long time in the die stagnation zone and oxidatively decomposes and carbonizes; the die is not cleaned in time during shutdown; high extrusion temperature accelerates carbonization
Solução
1)Flush the die with pure PE for 3-5min before shutdown to remove CMC residue; 2)Disassemble and clean the die immediately after shutdown; 3)Lower extrusion temperature by 5-10°C to reduce carbonization tendency; 4)Optimize die flow channel to reduce stagnation zone dead corners
Conclusão principal
Die carbon deposits are caused by thermal oxidation and untimely cleaning; PE flushing and timely cleaning are the key