Injection Molding 1 visualizações

DSTDP injection molded product ejector whitening

Fenómeno do problema
DSTDP injection molded product shows white marks at ejector pin positions, ejector whitening affecting appearance
Análise das causas
Ejector pin force too large causing local compression deformation and whitening; cooling time insufficient, product ejected before fully solidified; ejector pin area too small, stress concentration
Solução
1) Extend cooling time so the product is fully solidified before ejection; 2) increase ejector pin area, use ejector plate instead of small ejector pins; 3) reduce ejection speed to reduce impact force; 4) increase demolding draft to reduce ejection force
Conclusão principal
Ejector whitening is caused by excessive ejection force and insufficient cooling; increasing ejector pin area and extending cooling time are key