Processing Machinery
7 visualizações
DSTDP insufficient mixing
Fenómeno do problema
After DSTDP is compounded with filler/additives, dispersion uneven, local agglomeration
Análise das causas
Screw mixing section length insufficient; number of kneading blocks insufficient; feeding method improper, additives and DSTDP not fully contacted
Solução
1) Increase screw mixing section length to 3-4D; 2) increase number of kneading blocks; 3) additives added after the side feeding port to increase mixing time
Conclusão principal
Insufficient mixing is caused by improper screw design; increasing the mixing section is key
Isto foi útil?
0 pessoas acharam isto útil