Extrusion & Post 13 visualizações

Glass Fibre film poor printing adhesion

Fenómeno do problema
After Glass Fibre film printing, ink adhesion
Análise das causas
Glass Fibre surface polarity has poor affinity with ink; corona treatment effect decays fast; ink system not matched with Glass Fibre
Solução
1) Print immediately within 24h after corona treatment; 2) use Glass Fibre dedicated ink; 3) raise corona power to 15-20kW/m² to ensure surface tension >42mN/m; 4) flame treatment to assist surface polarization
Conclusão principal
Poor printing adhesion is caused by insufficient surface polarity; corona treatment and dedicated ink are key
Glass Fibre filmprinting adhesioncorona treatmentdedicated inksurface tension