Processing Machinery 7 visualizações

Glass Fibre difficult purging

Fenómeno do problema
Glass Fibre purging needs 2-3h, time-consuming, affecting product changeover efficiency
Análise das causas
Glass Fibre adhesion strong, forms firm adhesive layer on screw and barrel; Glass Fibre thermal stability poor, becomes sticky at high temperature, harder to remove
Solução
1) Before purging, flush with high-viscosity PE to carry away Glass Fibre residue; 2) reduce purging temperature below Glass Fibre softening point to reduce adhesion; 3) use dedicated purging compound
Conclusão principal
Difficult purging is caused by Glass Fibre strong adhesion; PE flushing and temperature reduction are key
Glass Fibredifficult purgingadhesionPE flushingdedicated purging compound