Injection Molding 6 visualizações

Glass Fibre injection multi-cavity unbalanced filling

Fenómeno do problema
Glass Fibre injection 8-cavity mold, each cavity fill amount differs ±15%, some cavities short shot, some flash
Análise das causas
Runner design unbalanced, each cavity runner length and resistance inconsistent; each cavity gate size inconsistent
Solução
1) Adopt balanced runner design to ensure each cavity runner equal length and equal resistance; 2) each cavity gate size precisely consistent ±0.01mm; 3) reduce injection speed to reduce resistance difference influence; 4) use mold flow analysis software to optimize runner design
Conclusão principal
Multi-cavity unbalanced filling is caused by runner design; balanced runner and mold flow analysis are key
Glass Fibre injectionmulti-cavity balancerunner designgate sizemold flow analysis