Material Analysis
14 visualizações
Glass Fibre large creep deformation
Fenómeno do problema
Glass Fibre product under long-term load creep >5%, exceeding 2% requirement
Análise das causas
Glass Fibre elastomer nature, creep large; molecular weight too low, creep resistance poor; not crosslinked, plastic flow large
Solução
1) Select high molecular weight grade; 2) slight crosslinking 0.3wt% DCP to reduce plastic flow; 3) add rigid filler to reduce creep
Conclusão principal
Large creep is caused by elastomer nature; slight crosslinking and rigid filler are key