MP length out of tolerance
Fenómeno do problema
MP product length deviation >±0.5mm, exceeding the tolerance
Análise das causas
MP shrinkage rate unstable, fluctuating ±0.5%; mold dimension design did not consider shrinkage compensation; insufficient cooling, dimensions not stabilized
Solução
1) precisely measure the MP shrinkage rate and compensate the mold; 2) fully cool to ensure dimensional stability; 3) annealing to eliminate post-shrinkage
Conclusão principal
length out of tolerance is caused by unstable shrinkage rate; precise shrinkage compensation is key