Extrusion & Post 13 visualizações

Analysis and Solution of crosslinking degree of PAA in adhesive during coating

Fenómeno do problema
When PAA produces adhesive by coating, abnormal performance related to crosslinking degree occurs.
Análise das causas
The main reason is improper setting of parameters in terms of crosslinking degree, leading to unstable processing.
Solução
Comprehensively solve the crosslinking degree problem from the perspective of equipment improvement.
Conclusão principal
The control of crosslinking degree of PAA is a key link in ensuring processing quality.