Injection Molding
7 visualizações
Optimization of the discoloration problem of PBD in '2079851475616104452
Fenómeno do problema
Polybutadiene PBD, as an elastomer toughening modifier or HIPS component, exhibited discoloration-related abnormalities during the '2079851475616104452 process.
Análise das causas
The molecular weight distribution of PBD affects processing; improper shear control leads to performance deterioration.
Solução
According to application requirements, optimize the compounding process to systematically solve the problem.
Conclusão principal
The core of PBD processing lies in structure control.
Isto foi útil?
0 pessoas acharam isto útil