Blow Molding 7 visualizações

Solution for mold temperature of calcium-zinc stabilizer in film '2079851475616104457

Fenómeno do problema
The calcium-zinc PVC system shows mold temperature-related abnormalities in the film '2079851475616104457 production stage, customers complain.
Análise das causas
The lubrication characteristic of calcium-zinc stabilizers produces mold temperature problems under specific working conditions.
Solução
From the formulation perspective, increase auxiliary stabilizers, combined with process optimization to solve it.
Conclusão principal
The mold temperature problem of the calcium-zinc system in the film '2079851475616104457 stage requires coordinated optimization of formulation and process.
calcium-zinc stabilizerfilm '2079851475616104457mold temperaturelubrication

Isto foi útil?

0 pessoas acharam isto útil