Material Drying 7 visualizações

Control of transparency abnormality in PEOX '2079851475616104458 packaging

Fenómeno do problema
During PEOX '2079851475616104458 production of packaging, the problem of not up to standard transparency occurs.
Análise das causas
Mainly due to the processing temperature deviating from the window +60-100°C, moisture content >0.1% exceeding the standard, and insufficient cooling.
Solução
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
Conclusão principal
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.