Injection Molding 2 visualizações

Extremely High Mold Temperature Requirement in LCP '2079851475616104452

Fenómeno do problema
LCP requires a mold temperature of 80-160°C or even higher to obtain good crystallization.
Análise das causas
LCP has a high melting point (>300°C) and a narrow crystallization temperature range, requiring a high-temperature mold to ensure sufficient crystallization to obtain the best performance.
Solução
Use an oil temperature machine or an electrically heated mold to reach the required mold temperature; the mold heating system needs to be specially designed for heat preservation.
Conclusão principal
The high mold temperature requirement of LCP is a major feature of its processing.
LCPmold temperaturecrystallizationoil temperature machineelectric heating