PC/ABS product weld line
Fenómeno do problema
Strength decreases and appearance is poor at the weld line of multi-gate products.
Análise das causas
When two streams of the PC/ABS two-phase alloy converge, fusion is poor, especially as the rubber phase in ABS hinders fusion.
Solução
Increase melt temperature 250-270°C and mold temperature 70-90°C; optimize gates to reduce weld lines.
Conclusão principal
PC/ABS weld lines are a common weakness in the alloy field.