Molds & Tooling
7 visualizações
PPS mold heating system design
Fenómeno do problema
PPS requires 140°C mold temperature, which is difficult to achieve with ordinary mold heating systems.
Análise das causas
The mold needs uniform heating to 140-150°C across all areas to prevent cold spots from causing poor local crystallization.
Solução
Design electric heating tube heating system + insulation board; zone temperature control and use infrared to detect temperature distribution.
Conclusão principal
PPS mold high-temperature uniformity is the foundation of product consistency.
Isto foi útil?
0 pessoas acharam isto útil