Injection Molding 2 visualizações

POE '2079851475616104452 cold slug marks

Fenómeno do problema
POE injection molded product shows cold slug marks near the gate
Análise das causas
Nozzle temperature too low causes residual material from the previous injection to cool and solidify in the nozzle; cold slug well design insufficient to hold cold slug; injection pressure insufficient
Solução
1) Raise nozzle temperature to 160-200°C; 2) Mold design with a sufficiently large cold slug well; 3) Ensure fresh melt at the nozzle front before each injection; 4) Increase injection pressure to push cold slug through the gate
Conclusão principal
Cold slug marks are caused by solidified residual material in the nozzle; raising nozzle temperature and cold slug well design are key
POE injectioncold slug marknozzle temperaturecold slug wellinjection pressure