Extrusion & Post 10 visualizações

POE extrusion pipe ovality exceeds standard

Fenómeno do problema
POE extruded pipe ovality >1.05, exceeding the 1.02 standard requirement
Análise das causas
Pipe cooling uneven, single-side cooling; sizing sleeve design unreasonable; haul-off clamping force uneven causing pipe deformation under pressure
Solução
1) Adopt annular spray cooling to ensure uniform cooling; 2) Optimize sizing sleeve inner diameter and taper design; 3) Multi-track uniform clamping haul-off; 4) Increase vacuum sizing section length to ensure full sizing
Conclusão principal
Ovality is caused by uneven cooling and clamping; annular cooling and uniform haul-off are key
POE pipeovalityannular coolingvacuum sizinguniform haul-off