POE internal black speck carbonization
Fenómeno do problema
POE product interior shows 0.1-0.5mm black speck carbonized material
Análise das causas
POE carbonized by prolonged heating in barrel dead corner zones; carbon deposit at the screw head; raw material impurities
Solução
1) Lower processing temperature to reduce carbonization; 2) Regularly clean screw and barrel; 3) Raw material filtration to remove impurities
Conclusão principal
Black specks are caused by thermal carbonization and carbon deposits; lowering temperature and regular cleaning are key