Extrusion & Post 15 visualizações

Melt flow rate mismatch of raw material for random copolymer polypropylene extrusion

Fenómeno do problema
After using a certain batch of raw material, extrusion process parameters need major adjustment and product quality fluctuates. MFR mismatch makes the original process parameters inapplicable, affecting production efficiency.
Análise das causas
(1) Raw material MFR is on the low side, resulting in high extrusion energy consumption and low output (2) Raw material MFR is on the high side, resulting in decreased product mechanical properties (3) Mixing raw materials of different grades results in inconsistent MFR (4) Raw material is stored for too long and MFR changes (5) MFR fluctuates greatly between raw material batches
Solução
(1) Select extrusion-grade grades with suitable MFR; random copolymer polypropylene extrusion usually selects MFR 0.3-5g/10min (2) Test MFR for each batch of raw material and match it with process requirements (3) Avoid mixing different grades; conduct tests first if mixing is necessary (4) Use raw materials within the shelf life (5) Appropriately increase barrel temperature when MFR is on the low side (6) Appropriately decrease barrel temperature when MFR is on the high side
Conclusão principal
MFR mismatch needs to be solved by selecting suitable grades and adjusting temperature parameters.
melt flow rategrade selectionextrusion gradeprocess adjustmentbatch testing