Extrusion & Post
14 visualizações
Melt flow rate mismatch of raw materials for random copolymer polypropylene pipe special material extrusion (Variant: mass production scenario)
Fenómeno do problema
After using a certain batch of raw material, the extrusion process parameters need to be greatly adjusted, and the product quality fluctuates.
The MFR mismatch makes the original process parameters inapplicable, affecting production efficiency.
In particular, in continuous mass production, this problem is more prominent and needs key attention.
Análise das causas
(1)The raw material MFR is low, the extrusion energy consumption is large, and the output is low
(2)The raw material MFR is high, and the mechanical properties of the product decrease
(3)Different grades of raw materials are mixed, and the MFR is inconsistent
(4)The raw material has been stored for too long, and the MFR has changed
(5)The MFR fluctuates greatly between batches of raw materials
(6)In continuous mass production, process parameter fluctuations or equipment status changes have aggravated this problem
Solução
(1)Select an extrusion grade with suitable MFR, random copolymer polypropylene pipe special material extrusion usually selects MFR 0.3-5g/10min
(2)Test the MFR of each batch of raw material and match it with the process requirements
(3)Avoid mixing different grades, and do a test first when mixing is necessary
(4)Use the raw material within the shelf life
(5)When the MFR is low, appropriately raise the barrel temperature
(6)When the MFR is high, appropriately lower the barrel temperature
(6)And establish standardized work instructions, with special attention to parameter stability in continuous mass production
Conclusão principal
MFR mismatch needs to be solved by selecting suitable grades and adjusting temperature parameters.
In different production scenarios, targeted preventive measures need to be taken.
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!