Screw design mismatch of random copolymer polypropylene pipe special material extruder
Fenómeno do problema
The product is unevenly plasticized, the output is low or the energy consumption is high, and the screw does not match the raw material characteristics.
The screw design directly affects the plasticization quality, output, and energy consumption.
Análise das causas
(1)The screw compression ratio does not match the density and melting characteristics of random copolymer polypropylene pipe special material
(2)The screw L/D ratio is insufficient, and the plasticizing section length is not enough
(3)The design of the transition section between the screw head and the die head is improper
(4)The screw mixing elements are not suitable for this material
(5)The screw thread depth design is improper
Solução
(1)Select a screw compression ratio suitable for random copolymer polypropylene pipe special material, generally 2.5-4.0
(2)The screw L/D ratio is at least 25:1 to ensure sufficient plasticization
(3)Optimize the transition section between the screw head and the die head to eliminate stagnant areas
(4)Select suitable mixing elements (pins, barriers, etc.) according to the material characteristics
(5)Ask professional screw designers to optimize the thread parameters according to the material characteristics
Conclusão principal
The screw design needs to match the material characteristics and product requirements, and a special screw needs to be customized if necessary.