Insufficient strength of PBT injection molded parts (unreinforced)
Fenómeno do problema
Pure PBT injection molded products easily break when stressed, and the strength does not meet the requirements.
Análise das causas
Pure PBT resin itself has limited strength and modulus (tensile strength about 55MPa), no reinforcing materials such as glass fiber are added, and there is internal stress.
Solução
Switch to glass fiber reinforced grades (30%GF tensile strength can reach more than 130MPa); optimize the molding parameters to reduce internal stress.
Conclusão principal
PBT engineering applications usually require glass fiber reinforcement to meet strength requirements.