Injection Molding
14 visualizações
Insufficient Bonding Force in PBT Two-Color '2079851475616104452
Fenómeno do problema
When PBT is two-color injection molded with other materials (such as TPE), the bonding force between the two layers is insufficient.
Análise das causas
The two materials are incompatible or the interfacial bonding force is weak; the temperature of the first-shot part is too low, so a molten bond cannot be formed during the second injection.
Solução
Select a compatible second-shot material; keep the first-shot part at a high temperature; consider interfacial bonding in the mold design.
Conclusão principal
PBT two-color '2079851475616104452 requires material matching and temperature management.
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!