Crystalline White Spots Near the Gate of PBT Injection-Molded Parts
Fenómeno do problema
White opaque areas appear near the gate of PBT products, with an obvious color difference from the main body.
Análise das causas
Shear-induced crystallization at the gate forms spherulites; rapid cooling causes incomplete crystal growth, resulting in whitening; the gate size is too small and the shear is large.
Solução
Increase the gate size to reduce shear; increase the mold temperature in this area; reduce the injection speed.
Conclusão principal
PBT gate white spots are the result of shear-induced crystallization.