Fenómeno do problema
Excessive drying of PC pellets (too high temperature or too long time) causes product discoloration and performance decline.
Análise das causas
Although PC requires strict drying, excessive drying causes thermal degradation and color darkening.
Solução
Strictly perform the drying at 120°C/4-6h; use timing and temperature control protection.
Conclusão principal
Excessive drying of PC is also harmful and requires precise control.