Material Drying
4 visualizações
Color darkening in PET extrusion pelletizing
Fenómeno do problema
After extrusion pelletizing of PET recycled material, pellet color obviously darkens (yellowing), IV value decreases.
Análise das causas
Extrusion temperature too high or residence time too long causes thermal degradation, residual moisture in recycled material causes hydrolysis, screw shear too strong generates shear heat.
Solução
Control extrusion temperature 260-280°C; fully dry recycled material; use low-shear screws; nitrogen protection in the hopper to prevent oxidation.
Conclusão principal
PET recycling pelletizing color and IV value control are key indicators of recycling quality.
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!