Extrusion & Post 7 visualizações

Excessive thermal shrinkage rate of PET biaxially stretched film

Fenómeno do problema
The thermal shrinkage rate of PET film exceeds the standard (longitudinal >3%, transverse >2%), causing inaccurate printing registration.
Análise das causas
Insufficient heat setting treatment after stretching (temperature on the low side or time insufficient); large draw ratio results in high internal stress; cooling is too fast.
Solução
Increase heat setting temperature to 200-230°C; increase setting time; appropriately reduce the draw ratio; control cooling rate.
Conclusão principal
PET film thermal shrinkage rate is dominated by the heat setting process.
PETfilmthermal shrinkageheat settingdraw ratio