Injection Molding
7 visualizações
Poor gloss of PET injection molded products
Fenómeno do problema
The surface gloss of PET injection molded products is insufficient, showing a matte or rough state.
Análise das causas
The mold surface roughness is poor and not polished to a mirror finish; melt temperature is on the low side and replication is poor; mold temperature is low with rapid cooling.
Solução
Polish the mold to a mirror finish Ra≤0.05μm; increase melt and mold temperature; strengthen drying; increase injection pressure and speed.
Conclusão principal
High gloss of PET products requires mirror molds, high-temperature processes and clean raw materials.
Isto foi útil?
0 pessoas acharam isto útil