Material Drying
7 visualizações
Degradation during PLA twin-screw extrusion granulation
Fenómeno do problema
Severe degradation and molecular weight decrease occur during PLA recycling granulation.
Análise das causas
The twin-screw shear is strong and the temperature is high, and PLA degrades quickly, especially when it contains moisture, hydrolysis and pyrolysis act together.
Solução
Use a low-shear screw configuration; strictly control the temperature at 160-180°C; fully dry the waste material.
Conclusão principal
PLA granulation is a technical difficulty for recycling.
Isto foi útil?
0 pessoas acharam isto útil