Injection Molding 7 visualizações

Glass fiber exposure (floating fiber) on the surface of glass fiber reinforced polyamide (general-purpose nylon) products

Fenómeno do problema
Glass fiber exposure (floating fiber) appears on the surface of glass fiber reinforced polyamide (general-purpose nylon) products, and the surface is rough with silver filaments
Análise das causas
(1)The glass fiber length is too long or the content is too high (2)The injection speed is low and the glass fiber is exposed following the flow orientation (3)The mold temperature is low and the glass fiber does not fuse well with the matrix (4)The barrel temperature is low, the melt flowability is insufficient, and the glass fiber is exposed (5)The interfacial bonding between the glass fiber and PA is not strong
Solução
(1)Optimize the glass fiber length and content (2)Appropriately increase the injection speed to reduce glass fiber orientation (3)Raise the mold temperature to the higher value of 60-90°C to improve fusion (4)Raise the barrel temperature to the higher value of 240-280°C (5)Add a coupling agent to improve the interfacial bonding
Conclusão principal
Glass fiber PA floating fiber needs to be addressed from injection speed and mold temperature
floating fiberglass fiberinjection speedcoupling agent

Isto foi útil?

0 pessoas acharam isto útil