Insufficient Welding/Fusion Strength of acrylonitrile-styrene copolymer Products
Fenómeno do problema
After the products are joined by hot plate welding, ultrasonic welding, etc., the welding strength is insufficient, and they break from the weld when stressed.
Análise das causas
(1)The welding temperature is low, and the material is not fully melted and fused
(2)The welding pressure is insufficient or the time is too short
(3)The welding surface is contaminated (oil, dust, etc.)
(4)The material contains moisture or additives affect the welding
(5)The welding surface is uneven, and the contact area is insufficient
Solução
(1)Optimize the welding temperature to the suitable range of acrylonitrile-styrene copolymer
(2)Increase the welding pressure and time
(3)Clean the welding surface before welding
(4)Fully dry the raw material and reduce the additive dosage
(5)Ensure the welding surface is flat
Conclusão principal
The welding strength is determined by the melt fusion quality.