Extrusion & Post 7 visualizações

Shell-core delamination of products

Fenómeno do problema
The product sounds dull when knocked, and separation of the skin layer and core layer is clearly visible on the cross-section
Análise das causas
Mold temperature is too low; the skin layer cools rapidly while the core layer is still flowing; the shrinkage rate difference between the two components is >0.5%; holding pressure switchover position is too early
Solução
Increase mold temperature to an appropriate range (determined by the matrix material); select blended components with similar shrinkage rates; delay holding pressure switchover to over 95% filling
Conclusão principal
Shell-core delamination is the result of the combined action of cooling shrinkage differences and holding pressure conditions
shell-core delaminationmold temperatureshrinkage rate differenceholding pressure switchovercooling